Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 66.0 MPa | 9570 psi | ILSS - Interlaminar; ASTM D2344 |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
Shear Strength | 66.0 MPa | 9570 psi | ASTM D732 |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | IS 867-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Shear Strength | 66.0 - 76.0 MPa | 9570 - 11000 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Shear Strength | 66.0 - 75.0 MPa | 9570 - 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Shear Strength | 66.0 MPa @Temperature 23.0 °C |
9570 psi @Temperature 73.4 °F |
ASTM D732 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer