Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 62.1 MPa | 9010 psi | Conditioned; ASTM D732 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Shear Strength | 62.1 MPa | 9010 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Shear Strength | 62.1 - 101 MPa | 9010 - 14600 psi | Average value: 85.4 MPa Grade Count:17 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |