Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 32.4 MPa @Temperature 23.9 °C |
4700 psi @Temperature 75.0 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 120 Aramid Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Shear Strength | 32.4 MPa | 4700 psi | Overlap, Distilled Water immersion for 30 days |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 32.4 MPa | 4700 psi | Overlap, Water Vapor, 49°C at 100% RH for 30 days |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 32.4 MPa | 4700 psi | Overlap, Etched Aluminum, 50% Antifreeze at RT for 30 days immersion, Cohesive Failure |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 32.4 MPa | 4700 psi | Aluminum, etched, Overlap, 30 day IPA soak, Cohesive Failure |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |
|||
Shear Strength | 32.4 MPa | 4700 psi | Aluminum, etched, Overlap, 30 day IPA soak, Cohesive Failure |
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of.. |
|||
Shear Strength | 32.4 MPa | 4700 psi | Interlaminar S23; ASTM D2344 |
Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |