Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 3.10 MPa | >= 450 psi | Lap |
Parker Chomerics CHO-BOND 1029 Conductive Adhesive CHO-BOND® 1029 is a highly conductive silicone adhesive, intended for bonding Chomerics’ conductive silicone EMI gaskets to electrically conductive substrates. It is a two-component, siliver-plate.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Plate Shear, W Direction, typ, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-11.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Shear Strength | >= 3.10 MPa | >= 450 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-78 - 3/16 - 6.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Shear Strength | >= 3.10 MPa | >= 450 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRP - 1/4 - 6.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, ABS |
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive 3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, PVC |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Shear Strength | 3.10 MPa @Temperature 66.0 °C |
450 psi @Temperature 151 °F |
Overlap |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Shear Strength | 3.10 MPa @Temperature 82.0 °C, Time 900 sec |
450 psi @Temperature 180 °F, Time 0.250 hour |
Aluminum Overlap |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, Gasoline for 14 days, Cohesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 3.10 MPa @Temperature 32.0 °C |
450 psi @Temperature 89.6 °F |
Overlap, Aluminum, 90% RH, Adhesive Failure |
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, Pine, Substrate/Cohesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, MDF, Cohesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 3.10 MPa @Temperature 32.0 °C |
450 psi @Temperature 89.6 °F |
Overlap, Aluminum, 90% RH, Adhesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, Isopropyl Alcohol Wipe surface prep, ABS PVC |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 3.10 MPa | 450 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |