Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 3.03 MPa
>= 440 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 3.03 MPa
440 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 3.03 MPa
440 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 3.03 MPa
440 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 3.03 MPa
440 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP/F50 - 5.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength >= 3.03 MPa
>= 440 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR III 1/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 3.03 MPa
440 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength >= 3.03 MPa
>= 440 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® CR-PAA™ 1/8-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 3.03 MPa

@Temperature 117 °C,
Time 4.406e+6 sec
440 psi

@Temperature 243 °F,
Time 1224 hour
Overlap, Cured for 7 days at 24°C
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 3.03 MPa
440 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M