Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 2.21 MPa | >= 320 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Shear Strength | 2.21 MPa | 320 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 1/4-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 2.21 MPa | >= 320 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRH-10/F50 - 5.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglass cloth reinforc.. |
|||
Shear Strength | 2.21 MPa | 320 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-327 - 3/16 - 4.5 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Strength | 2.21 MPa | 320 psi | Bond, Al to Al |
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper.. |
|||
Shear Strength | 2.21 MPa | 320 psi | Lap Shear Strength; ASTM D1002 |
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Shear Strength | 2.21 MPa | 320 psi | Overlap, Isopropyl Alcohol Wipe surface prep, ABS PVC |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 2.21 MPa | 320 psi | Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 2.21 MPa | 320 psi | Overlap, Aluminum -120 frit sandpaper |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 2.21 MPa | 320 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |