Polymer Property : Shear Strength = 2999 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 20.68 MPa
2999 psi
Ritelok RT09 Bearing Mount Adhesive
Anaerobic. Low viscosity threadlocker for tight tolerances. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Shear Strength 20.68 MPa
2999 psi
Ritelok RT20 High Temperature Retainer
Anaerobic. High temp, retainer for auto/marine cylinder liners & heat exchange tubes. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Shear Strength 20.68 MPa
2999 psi
Ritelok RT40 Adhesive
Anaerobic. High strength, medium viscosity retainer for rotors to shafts/bushings to sleeves. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant