Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 0.200 MPa | >= 29.0 psi | ASTM C273 |
Parabeam Industrie Paraglass 12 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Strength | 0.200 MPa | 29.0 psi | Typical; ASTM C273 |
Parabeam Industrie Paraglass 12 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Strength | 0.200 MPa | 29.0 psi | Typical; ASTM C273 |
Parabeam Industrie Paraglass 15 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Strength | 0.200 - 0.300 MPa | 29.0 - 43.5 psi | Average value: 0.290 MPa Grade Count:5 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Shear Strength | 0.200 - 0.300 MPa | 29.0 - 43.5 psi | Average value: 0.290 MPa Grade Count:5 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Shear Strength | 0.200 MPa | 29.0 psi | |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Shear Strength | >= 0.200 MPa | >= 29.0 psi | ASTM C273 |
Parabeam Industrie Paraglass 10 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |