Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.93 MPa | 280 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR III 3/8-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Plate Shear, L Direction, typ, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, L Direction, min, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-327 - 3/8 - 4.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, W Direction, min, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 3/8 - 7.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRP - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 3/8 - 6.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP/F35 - 4.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR III 3/16-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/16-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Overlap, ABS |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Shear Strength | 1.93 MPa | 280 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Shear Strength | 1.93 MPa | 280 psi | Overlap, Polycarbonate |
3M Scotch-Weld™ DP405 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, L Direction, min, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |
|||
Shear Strength | >= 1.93 MPa | >= 280 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 3/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |