Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.0 MPa @Temperature 81.0 - 83.0 °C |
2760 psi @Temperature 178 - 181 °F |
Etched Aluminum Overlap, Tap Water Immersion for 30 days |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |