Mechanical Properties Metric English Comments
Shear Strength 18.3 MPa
2650 psi
Overlap, CRS/CRS after 7 days of Immersion in Toulene
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 18.3 MPa
2650 psi
Overlap, CRS/CRS after 7 days of Immersion in IPA
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 18.3 MPa
2650 psi
Overlap, Toluene for 14 days, Cohesive Failure
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 18.3 MPa
2650 psi
Overlap, Etched Al, 100% RH at 49°C for 30 days
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..