Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 16.9 MPa | 2450 psi | Overlap, Stainless Steel/Stainless Steel |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 16.9 MPa | 2450 psi | Overlap, Brass/Brash |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 16.9 MPa @Temperature 23.0 °C |
2450 psi @Temperature 73.4 °F |
Overlap, Green FRP, Adhesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 16.9 MPa | 2450 psi | Overlap, Oak, Substrate/Cohesive Failure |
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |