Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 16.5 MPa | 2400 psi | |
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Shear Strength | >= 16.5 MPa | >= 2400 psi | Lap, Al/Al |
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable .. |
|||
Shear Strength | >= 16.5 MPa | >= 2400 psi | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Shear Strength | 16.5 MPa @Temperature 24.0 °C |
2400 psi @Temperature 75.2 °F |
Overlap, Steel Solvent Wipe; ASTM D1002-72 |
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M |
|||
Shear Strength | 16.5 - 17.2 MPa | 2400 - 2500 psi | CRS Overlap |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Shear Strength | 16.5 MPa | 2400 psi | Overlap, Aluminum; ASTM D1002-64 |
3M Scotch-Weld™ CA9 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting version of CA8 for wire tacking and coil terminating. Meets CID A-A-3097, Type II, C.. |
|||
Shear Strength | 16.5 MPa | 2400 psi | Overlap, Stainless Steel MEK/abrade/MEK |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 16.5 MPa @Temperature 24.0 °C |
2400 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 16.5 MPa @Temperature 24.0 °C |
2400 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 16.5 MPa | 2400 psi | Overlap, CRS - with Ferrocote 6130 Draw Lube, Cohesive failure/Adhesive Failure; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 16.5 MPa | 2400 psi | ASTM D1002-94 |
Aremco Aremco-Bond™ 2200 High Performance Epoxide Glass Fiber- and Kevlar-Reinforced, Epoxy-Novolac; High Strength, Excellent Abrasion and Corrosion Resistance |
|||
Shear Strength | 16.5 MPa | 2400 psi | Overlap, Oak, Substrate/Cohesive Failure |
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 16.5 MPa | 2400 psi | Overlap, Aluminum; ASTM D1002-64 |
3M Scotch-Weld™ CA7 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3.. |
|||
Shear Strength | 16.5 MPa @Temperature 24.0 °C |
2400 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 16.5 MPa | 2400 psi | Overlap, Cold Rolled Steel (oily) |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 16.5 MPa | 2400 psi | Lap, Alum to Alum |
Atom Adhesives AA-BOND 2170 Epoxy Adhesive AA-BOND 2170 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, kapton or almost any thermoplastic substrate. A.. |
|||
Shear Strength | 16.5 MPa @Temperature 24.0 °C |
2400 psi @Temperature 75.2 °F |
Aluminum Overlap; ASTM D1002 |
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar.. |
|||
Shear Strength | 16.5 MPa @Temperature 24.0 °C |
2400 psi @Temperature 75.2 °F |
Aluminum Overlap; ASTM D1002 |
3M Scotch-Weld™ DP 3501 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi.. |