Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.0 MPa @Thickness >=5.00 mm |
2180 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; IEC/EN 60893-2 5.5 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Sheets Description: Electrical and electrotechnical applications. Suitable as high-frequency insulation on account of its dielectric loss. Used as, among other things, an insulation material in large induc.. |
|||
Shear Strength | >= 15.0 MPa | >= 2180 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF WV 201 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Shear Strength | >= 15.0 MPa | >= 2180 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF WV 202 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical and electrical applications. Good electrical properties under normal humidity.Information provided by Hippe. |
|||
Shear Strength | >= 15.0 MPa | >= 2180 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF WV 303 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical applications. Good mechanical properties.Information provided by Hippe. |
|||
Shear Strength | >= 15.0 MPa | >= 2180 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Shear Strength | 15.0 MPa | 2180 psi | Short Beam |
COI Ceramics Nextel™ AS-N610 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Shear Strength | 15.0 - 26.0 MPa | 2180 - 3770 psi | tensile; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thin Cyanoacrylate Adhesive BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas.. |
|||
Shear Strength | 15.0 - 22.0 MPa | 2180 - 3190 psi | tensile; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |