Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 12.11 MPa | 1756 psi | Lap |
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No.. |