Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Haysite H260 Polyester Laminate Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Shear Strength | 103 MPa | 14900 psi | |
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m.. |
|||
Shear Strength | 103 MPa | 14900 psi | |
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil.. |