Mechanical Properties Metric English Comments
Shear Strength 100 MPa

@Thickness 15.7 mm
14500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..
Shear Strength 100 MPa
14500 psi
ASTM D732
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)
Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product.
Shear Strength 100 MPa

@Thickness 15.7 mm
14500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP322 Cotton Fabric
Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320..
Shear Strength 100 MPa

@Thickness 15.7 mm
14500 psi

@Thickness 0.620 in
ASTM D732
Industrial Laminates/Norplex NP325 Cotton Fabric
Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500".
Shear Strength 100 MPa
14500 psi
In-Plane Shear, Dry/RT; AiTM 1.0002
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System
HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process...
Shear Strength 100 - 120 MPa
14500 - 17400 psi
2mm/min.; IS 867-1963
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown..