Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 10.0 MPa | >= 1450 psi | Polycarbonate; ASTM D1002/DIN 53283 |
Palm Labs Adhesives TURBO FUSE METHYL FOR METALS (75-95 Viscosity) Rapid Bonding Adhesive Palm Lab's Methyl Cyanoacrylate is a one component rapid bonding adhesive ideal for metal surfaces. TURBO FUSE METHYL’s advanced formula is designed to polymerize instantly by absorbing surface moi.. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Shear Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | Cured; ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 130PR PLASTIC & RUBBER (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130PR PLASTIC & RUBBER’S advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Shear Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | Cured; ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 130PR PLASTIC & RUBBER (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130PR PLASTIC & RUBBER’S advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | ISO 10123; Compressive, Steel pins and collars |
Palm Labs Adhesives TURBO-LOCK SERIES 12 Anaerobic Thread Locking Compound TURBO-LOCK 12 SERIES is a fast curing, medium to high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water,.. |
|||
Shear Strength | 10.0 - 20.0 MPa | 1450 - 2900 psi | Average value: 15.0 MPa Grade Count:8 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information.. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 202 Cellulose Paper Reinforced Phenolic Resin - Sheet High voltage applications at power frequencies. High electric strength under oil. Good electrical strength in air under normal humidity.Information provided by Hippe. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 203 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe PF CP 207 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions. Improved .. |
|||
Shear Strength | >= 10.0 MPa | >= 1450 psi | ABS; ASTM D1002/DIN 53283 |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |
|||
Shear Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | neoprene rubber; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thin Cyanoacrylate Adhesive BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas.. |
|||
Shear Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | etched aluminum; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thin Cyanoacrylate Adhesive BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas.. |
|||
Shear Strength | 10.0 MPa | 1450 psi | Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 10.0 MPa | 1450 psi | Overlap, EC 3924 Primed Al/HDPE (non-abraded Al), Cohesive Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 10.0 MPa | 1450 psi | Overlap, Gel Coat (3/16" thick), Substrate Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 10.0 MPa | 1450 psi | Overlap, 71°C soak for 14 days, Mixed Mode of AF&CF |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | neoprene rubber; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |
|||
Shear Strength | 10.0 - 15.0 MPa | 1450 - 2180 psi | acrylics; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |
|||
Shear Strength | 10.0 MPa @Temperature 93.0 °C |
1450 psi @Temperature 199 °F |
Overlap, Etched Alum/Etched Alum |
3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |