Mechanical Properties Metric English Comments
Shear Strength >= 0.900 MPa
>= 131 psi
ASTM C273
Parabeam Industrie Paraglass 3 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Strength 0.900 MPa
131 psi
Plate Shear, L direction
Hexcel® HexWeb® CRF-1/2-ACG-.003-2.6 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..
Shear Strength 0.900 MPa
131 psi
Plate Shear, W direction
Hexcel® HexWeb® CRF-3/8-ACG-.003-3.7 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..
Shear Strength >= 0.900 MPa
>= 131 psi
ISO 1922
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Shear Strength 0.900 MPa
131 psi
average; ISO 1922
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Shear Strength >= 0.900 MPa
>= 131 psi
ISO 1922
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Shear Strength 0.900 MPa
131 psi
ASTM C273
3A Composites Core Materials AIREX® PXw.320 Fiber-Reinforced Structural Foam Panel