Polymer Property : Shear Strength = 1300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 8.96 - 11.0 MPa
1300 - 1600 psi
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.
Shear Strength 8.96 - 12.4 MPa
1300 - 1800 psi
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works.
Shear Strength 8.96 MPa
1300 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Phenolic
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 8.96 MPa
1300 psi
Overlap, Galvanized Steel
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Shear Strength 8.96 MPa
1300 psi
Overlap, PVC, Substrate Failure
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 8.96 MPa
1300 psi
Overlap, ABS, Substrate Failure
3M Scotch-Weld™ DP8805NS Low Odor Acrylic Adhesives
3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and ..
Shear Strength 8.96 MPa
1300 psi
Overlap, ABS, Substrate Failure
3M Scotch-Weld™ DP8810NS Low Odor Acrylic Adhesives
3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and ..
Shear Strength 8.96 MPa
1300 psi
Overlap, FRP (red) (IPA/abrade/IPA) - Substrate Failure; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Shear Strength 8.96 MPa

@Temperature 32.0 °C
1300 psi

@Temperature 89.6 °F
Overlap, Plywood, 90% RH, Substrate Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 8.96 MPa
1300 psi
Overlap, Cold Rolled Steel
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s..
Shear Strength 8.96 MPa

@Temperature 82.0 °C,
Time 900 sec
1300 psi

@Temperature 180 °F,
Time 0.250 hour
Aluminum, etched, Overlap, Adhesive Failure
3M Scotch-Weld™ LSB60NS Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60NS is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of..
Shear Strength 8.96 MPa
1300 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, SBR/Steel
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 8.96 MPa
1300 psi
cured, grit-blasted steel; ASTM D1002
3M Scotch-Weld™ RT3500B Rubber-Toughened Instant Adhesive
3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon..