Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 0.827 MPa | >= 120 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 5/32-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, W Direction |
Hexcel® HexWeb® HRH-36 - 1/8 - 3.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-36 - 3/16 - 2.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-78 - 1/4 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP - 3/8 - 2.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP - 3/8 - 3.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 0.827 MPa | >= 120 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Overlap, Neoprene Rubber; ASTM D1002-64 |
3M Scotch-Weld™ CA100 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-peel and impact strength and high thermal shock and heat resistance.Information provided by 3M.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Neoprene/Steel |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 0.827 MPa | 120 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 3/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |