Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 75.0 MPa @Temperature 75.0 °C |
10900 psi @Temperature 167 °F |
In-Plane, Wet; EN6031 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Shear Strength | 75.0 MPa | 10900 psi | In-Plane, RT, Dry; EN6031 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |
|||
Shear Strength | 75.0 MPa | 10900 psi | ILSS; EN2563 |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm Fiber mass: 150 g/m2Information provided by HexCel |
|||
Shear Strength | 75.0 - 80.0 MPa | 10900 - 11600 psi | IS 867-1963 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Shear Strength | >= 75.0 MPa | >= 10900 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Shear Strength | 75.0 - 90.0 MPa | 10900 - 13100 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |