Mechanical Properties Metric English Comments
Shear Strength 7.067 MPa
1025 psi
Overlap, HDPE/Galvanealed, Substrate Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.067 MPa
1025 psi
Overlap, HDPE/CRS, Adhesive/Cohesive Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.067 MPa
1025 psi
Overlap, NaOH for 14 days, Substrate Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.067 MPa
1025 psi
Overlap, Antifreeze Coolant for 14 days, Substrate Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.067 MPa

@Temperature 66.0 °C
1025 psi

@Temperature 151 °F
Overlap, Green FRP, AF/CF
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 7.067 MPa
1025 psi
Overlap, ED-5000 E-Coated CRS/HDPE, Adhesive Failure
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
Shear Strength 7.067 MPa
1025 psi
Overlap, Acrylic, Substrate Failure
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Shear Strength 7.067 MPa
1025 psi
Overlap, PC, Substrate Failure
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..