Mechanical Properties Metric English Comments
Shear Strength 55.2 - 82.7 MPa
8000 - 12000 psi
Average value: 67.3 MPa Grade Count:4
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Shear Strength 68.9 - 82.7 MPa
10000 - 12000 psi
ASTM D732
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..