Mechanical Properties Metric English Comments
Shear Strength 26.2 - 124 MPa

@Temperature -55.0 - 177 °C
3800 - 18000 psi

@Temperature -67.0 - 351 °F
Average value: 57.4 MPa Grade Count:22
Overview of materials for Epoxy/Carbon Fiber Composite