Polymer Property : Shear Strength = 12.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 10.3 - 12.4 MPa
1500 - 1800 psi
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works.
Shear Strength 10.3 - 12.4 MPa
1500 - 1800 psi
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works.
Shear Strength 8.96 - 12.4 MPa
1300 - 1800 psi
ITW Plexus Plexusâ„¢ MA550 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent marine adhesive, UV stable.Information provided by Illinois Tool Works.