Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.62 - 10.7 MPa | 1250 - 1550 psi | |
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g.. |