Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 91.5 MPa | 13300 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Shear Strength | 91.5 MPa | 13300 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Shear Strength | 91.5 MPa | 13300 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Shear Strength | 91.5 MPa | 13300 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |