Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 83.0 MPa | 12000 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Shear Strength | 83.0 MPa | 12000 psi | ASTM D732 |
Glastic Laminates/Shapes 1580 Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements. |
|||
Shear Strength | 83.0 MPa | 12000 psi | 0º, ILSS (Short Beam), RT, Dry; EN2563 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Shear Strength | 83.0 MPa @Temperature 23.0 °C |
12000 psi @Temperature 73.4 °F |
DAM; ASTM D732 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |