Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.101 MPa | 1175 psi | Overlap, 71°C water soak for 14 days, Cohesive Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 8.101 MPa | 1175 psi | Overlap, 71°C water soak for 14 days, Cohesive Failure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |