Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 79.3 MPa @Thickness 15.7 mm |
11500 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP629 Paper Base Laminate Description: It is a paper-phenolic high-pressure laminate. It is intended primarily for mechanical applications and is suitable for electrical applications as well. Thickness Tested: 0.062", 0.125".. |
|||
Shear Strength | 79.3 MPa @Thickness 15.7 mm |
11500 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP843 Paper Base Laminate Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through.. |
|||
Shear Strength | 79.3 MPa | 11500 psi | Short Beam; ASTM D5528-07 |
Zyvex Performance Materials Arovex™ 180 Carbon Nanotube Strengthened Prepreg Arovex® 180 Prepreg is a 180°F (82°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Arovex 180 resin contains an optimum level of carbon nanotub.. |