Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 52.4 MPa @Temperature 23.9 °C |
7600 psi @Temperature 75.0 °F |
Short-Beam, Dry; Oven Cure 275°F, 90 min; ASTM D2344 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Shear Strength | 52.4 MPa | 7600 psi | ASTM D732 |
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet) |
|||
Shear Strength | 52.4 MPa | 7600 psi | Ultimate; ASTM D3846 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex.. |
|||
Shear Strength | 52.4 MPa @Temperature 22.8 °C |
7600 psi @Temperature 73.0 °F |
Ultimate; ASTM D3846 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Shear Strength | 52.4 - 62.1 MPa | 7600 - 9000 psi | ASTM D732 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |