Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.50 MPa | 508 psi | average; ISO 1922 |
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Shear Strength | 3.50 MPa | 508 psi | ASTM C273 |
3A Composites Core Materials AIREX® PXc.320 Fiber-Reinforced Structural Foam AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu.. |