Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 206 MPa | 29900 psi | In Plane; ASTM D5379 |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |