Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.45 MPa | 355 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 2.45 MPa | 355 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRP/OX - 3/8 - 5.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | 2.45 MPa | 355 psi | Plate Shear, L Direction, typ, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Designation: Material-Cell Size-Density.Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the.. |
|||
Shear Strength | 2.45 MPa | 355 psi | Overlap, Teak, 50% RH |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |