Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 18.0 MPa | >= 2610 psi | ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Shear Strength | 18.0 - 28.0 MPa | 2610 - 4060 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Shear Strength | 18.0 - 28.0 MPa | 2610 - 4060 psi | Tensile, (Cured State) |
Palm Labs Adhesives Turbo Fuse Series 130SI Surface Insensitive (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Shear Strength | >= 18.0 MPa | >= 2610 psi | etched aluminum; ASTM D1002/DIN 53283 |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |
|||
Shear Strength | 18.0 - 28.0 MPa | 2610 - 4060 psi | tensile; ASTM D1002/DIN 53283 |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |