Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1207 MPa | 175100 psi | |
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Shear Strength | 1207 MPa | 175100 psi | |
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |