Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 12.0 MPa | >= 1740 psi | ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Shear Strength | 12.0 - 117 MPa | 1740 - 17000 psi | Average value: 83.9 MPa Grade Count:8 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Shear Strength | 12.0 MPa | 1740 psi | |
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by e.. |
|||
Shear Strength | 12.0 MPa | 1740 psi | |
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy .. |
|||
Shear Strength | >= 12.0 MPa | >= 1740 psi | Parallel to laminations; IEC 1212-2 5.6 |
Hippe EP PC 301 Woven Polyester Cloth Reinforced Epoxy Resin - Sheet Used in electrical and mechanical applications. Good resistance to SF6.Information provided by Hippe. |
|||
Shear Strength | >= 12.0 MPa | >= 1740 psi | polycarbonate; ASTM D1002/DIN 53283 |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |