Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 103 MPa | 15000 psi | ASTM D732 |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
Shear Strength | 103 MPa | 15000 psi | ASTM D732 |
Quantum PEI - Ultem® Information provided by Quantum Advanced Engineering Plastics |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Shear Strength | 103 MPa | 15000 psi | ASTM D732 |
Quadrant EPP Duratron® PEI U1000 Extruded Unfilled Polyetherimide (ASTM Product Data Sheet) |
|||
Shear Strength | 103 MPa | 15000 psi | |
XP Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Shear Strength | 103 MPa | 15000 psi | |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Shear Strength | 103 MPa @Thickness 15.7 mm |
15000 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP610 Paper Base Laminate Description: Phenolic paper based grade for mechanical applications. Good tensile, compressive and flexural strength. Primarily a machining material, but may be hot punched up to .093" thick.Thickne.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Haysite H260 Polyester Laminate Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g.. |
|||
Shear Strength | 103 MPa | 14900 psi | ASTM D732 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Shear Strength | 103 MPa | 14900 psi | |
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m.. |
|||
Shear Strength | 103 MPa | 14900 psi | |
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil.. |
|||
Shear Strength | 103 MPa | 15000 psi | Ultimate |
Ensinger TECAPEI® made from Ultem® 1000 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Shear Strength | 103 MPa | 15000 psi | ASTM D732 |
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |