Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 10.86 MPa | 1575 psi | Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 10.86 MPa | 1575 psi | Overlap, EC 3924 Primed CRS (non-abraded CRS), Cohesive Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |