Polymer Property : Shear Strength = 1.45 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 1.45 - 41.9 MPa
210 - 6080 psi
Average value: 19.2 MPa Grade Count:20
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..
Shear Strength 1.45 MPa
210 psi
Shin-Etsu Silicones KE-347TUV Silicone, RTV Coating
Information Provided by Shin-Etsu Silicones of America, Inc.
Shear Strength >= 1.45 MPa
>= 210 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10 - 1/8- 8.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 1.45 MPa
210 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-327 - 3/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 1.45 MPa
210 psi
Plate Shear, W Direction
Hexcel® HexWeb® HRH-36 - 1/8 - 4.5 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Strength >= 1.45 MPa
>= 210 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP - 3/16 - 4.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 1.45 MPa
210 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 3.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength >= 1.45 MPa
>= 210 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRP - 3/8 - 6.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength >= 1.45 MPa
>= 210 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRP/OX - 1/4 - 4.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength >= 1.45 MPa
>= 210 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP/OX - 3/8 - 5.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 1.45 MPa
210 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/8-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 1.45 MPa
210 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 3/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 1.45 MPa
210 psi
Plate Shear, L direction
Hexcel® HexWeb® CRF-3/8-ACG-.003-3.7 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..
Shear Strength 1.45 MPa
210 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 1.45 MPa
210 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..