Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.28 MPa | 186 psi | ribbon direction |
Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material Construction: ±45° Quartz. Fiber: Astroquartz II. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures. It is expected that it will b.. |
|||
Shear Strength | 1.28 MPa | 185 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/8 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 1.28 MPa | 185 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/4 - 3.1 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 1.28 MPa | 185 psi | silicone property; ASTM D1002 |
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Shear Strength | 1.28 MPa | 185 psi | silicone property; ASTM D1002 |
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Shear Strength | 1.28 MPa | 185 psi | Lap Shear Strength; ASTM D1002 |
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S.. |
|||
Shear Strength | 1.28 MPa | 185 psi | Lap Shear Strength; ASTM D1002 |
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val.. |
|||
Shear Strength | 1.28 MPa | 185 psi | Overlap, Pine, 50% RH |
3M 4200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an.. |