Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.448 MPa | 65.0 psi | Plate Shear, W Direction |
Hexcel® HexWeb® ACG®-3/4 Honeycomb Aluminum Commercial Grade HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. .. |
|||
Shear Strength | >= 0.448 MPa | >= 65.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.448 MPa | 65.0 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10/OX - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Strength | 0.448 MPa | 65.0 psi | Plate Shear, L Direction |
Hexcel® HexWeb® HRH-36/OX - 3/16 - 2.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Shear Strength | >= 0.448 MPa | >= 65.0 psi | Plate Shear, W Direction, min |
Hexcel® HexWeb® HRP/F50 - 3.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Shear Strength | 0.448 MPa | 65.0 psi | Plate Shear, L Direction |
Hexcel® HexWeb® ACG®-1 Honeycomb Aluminum Commercial Grade HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. .. |
|||
Shear Strength | 0.448 MPa | 65.0 psi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |