Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 738 MPa | 107000 psi | ASTM D790 |
LyondellBasell Plexar® PX2246 Extrudable Tie-Layer Resin - Anhydride Modified HDPE General DescriptionPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resin.. |