Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 420 MPa | 60900 psi | ASTM D638 |
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp.. |