Polymer Property : 1% Secant Modulus = 1320 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 1320 MPa
191000 psi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M5562 High Density Polyethylene
ApplicationsALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include noz..