Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.89 g/micron | 73.3 g/mil | ASTM D1709 |
Westlake EN1807AA Low Density Polyethylene WESTLAKE polyethylene EN1807 is a fractional-melt low- density formulation suggested for film applications requiring high impact strength, high tear strength, and very good optical properties, such .. |