Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.63 g/micron | 66.7 g/mil | ASTM D1709 |
Westlake EN923 Low Density Polyethylene Westlake Polyethylene EN923 is a low density formulation suggested for film applications where enhanced processability and high clarity are required. It is characterized by good tear strength, impa.. |