Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 12.6 g/micron | 320 g/mil | 73°F; ASTM D3029 |
Spartech SP-3810 TPO/TPE Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Dart Drop | 12.6 g/micron | 320 g/mil | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Vytek™ V208A3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |