Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 11.3 g/micron | 288 g/mil | F50; ASTM D1709 |
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and.. |